Watched a guy float a whole driveway in Fargo with a magnesium trowel while I stood there with my steel one
Two summers back I was on a crew pouring a 24 by 30 driveway in Fargo and this older finisher named Duane showed up with a mag float and nothing else. I figured he was just warming up. He worked that whole slab with it, edge to edge, and I kept waiting for him to switch. He never did. The finish came out smoother than anything I'd ever turned with steel, no burn marks, no swirls. I asked him why and he just said the mag gives you a little forgiveness when the sun starts working against you. Now I keep one on the truck and reach for it way more than I used to. Curious what the rest of you float with on a hot day, steel or mag, and why?